August 2017

Journal

Effect of Loading History on Stress Corrosion Cracking of 7075-T651 Aluminum Alloy in Saline Aqueous Environment

By:
Kalnaus, Sergiy ; Zhang, Jixi; Jiang, Yanyao; Behrooz, Majid
Journal Name:
Metallurgical and Materials Transactions A
Page Number:
448-460
Volume:
42
Issue Number:
2
Publication Date:
August 18, 2017
View DOI Listing:
https://doi.org/10.1007/s11661-010-0419-8