December 2023

Conference Paper

In Situ Transmission Electron Microscopy Study on the Deformation Responses of Additively Manufactured Multiphase Ni-based Superalloy

By:
Kirka, Michael M; Unocic, Kinga A; Guo, Qianying
Journal Name:
Microscopy and Microanalysis
Page Number:
1-4
Volume:
NA
Issue Number:
NA
Publication Date:
December 27, 2023
Conference Name:
Microscopy and Microanalysis 2020 Meeting
Conference Location:
Milwaukee, Wisconsin, United States of America
Conference Sponsor:
Microscopy Society of America, Microanalysis Society
View DOI Listing:
https://doi.org/10.1017/S1431927620019571