Measuring the constitutive behavior of viscoelastic solids in the time and frequency domain using flat punch nanoindentation

By:
Herbert, E.; Oliver, W.; Lumsdaine, A.; Pharr, George M
Journal Name:
Journal of Materials Research
Page Number:
626-637
Volume:
24
Issue Number:
3
Publication Date:
August 27, 2012
View DOI Listing:
https://doi.org/10.1557/JMR.2009.0089