July 2008

Journal

Reactive Wetting of an Iron-Based Superalloy MSA2020 and 316 Stainless Steel by Molten Zinc Alloy

By:
Liu, Xingbo ; Xu, Jing ; Bright, Mark A; Hemrick, James G; Barbero, Ever J
Journal Name:
Metallurgical and Materials Transactions A
Page Number:
1382-1391
Volume:
39A
Issue Number:
6
Publication Date:
July 8, 2008
View DOI Listing:
https://doi.org/10.1007/s11661-008-9501-x